Hi All Need some suggestions on how to handle solderjoint issue (How to tweak to pass TMCL1000 cycles- 0 to 100C) on QFN packages ( 5 x 6 x 1.0 mm with 8 pins). Finish is Pure Sn Board is 16 layers 3.2 mm, HASL finish. Does someone had an experience to share? thanks ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________