I just heard a very good paper at APEX about this very subject a few hours ago: The Relationship Between Backward Compatible Assembly, Microstructure, and Component Warpage on the Thermal Fatigue Reliability of an Extremely Large Ball Grid Array Richard Coyle, Alcatel-Lucent Karen Tellefsen - Electrical Testing [log in to unmask] 908-791-3069 [TN] BGA Reverse Backwards Compatibility Rivera, Raye to: TechNet 03/01/2012 03:09 PM Sent by: TechNet <[log in to unmask]> Please respond to TechNet E-Mail Forum, "Rivera, Raye" Hello TechNet Gurus. I have seen lots of discussion and studies on the reliability of using BGAs with SAC solder balls on an assembly with SnPb paste. Many people are interested in this topic because of backwards compatibility issues when SnPb BGAs aren't available. At the risk of oversimplifying a complex topic, I understand this can be successful using a backward compatibility thermal profile such as the one shown on Figure 8-20 of IPC-7095B to ensure complete melting of both types of solder. Of course we must take care that the profile does not exceed the temperature limitations of the SnPb paste. Is anyone aware of any study done on the reverse situation? That is, SnPb BGAs used with SAC solder paste and a SAC thermal profile? I would think it would be at least as reliable as the above situation. We definitely get complete melting and the temperature profile is correct for the SAC solder paste chemistry so we are not as concerned about holding a narrow process window. This is not just academic curiosity on my part. We have some prototype boards built with SnPb BGAs SAC paste, and SAC profile. They are not for sale to customers, but some of our engineers are of the opinion that any mixed process joint is suspect. I'd like to find some data on the topic. I hope everyone is enjoying Apex. Best regards, Raye Rivera QA Manager * Canoga Perkins 20600 Prairie Street * Chatsworth * CA 91311-6008 818-678-3872 * [log in to unmask] ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________