OOPS. I responded directly to Mike not Technet. Sorry Mike. Brs,Gerry From: [log in to unmask] To: [log in to unmask] Subject: RE: [TN] under-mask cleanliness of large panel Date: Sat, 3 Mar 2012 04:27:06 -0500 I think Mike has the correct answer. This way you can at least run a dynamic extraction if your ROSE equipment does this (it should). Another alternative but very tricky on such a large panel is to perform a "bagged extraction" per the IPC procedure (procdure number escapes me) and either run Ion Chromatography (preferably) or run the solution through your ROSE equipment. Brs, Gerry > Date: Fri, 2 Mar 2012 22:50:32 +0000 > From: [log in to unmask] > Subject: Re: [TN] under-mask cleanliness of large panel > To: [log in to unmask] > > One of the original reasons for the introduction of machines was the > difficulty of doing repeatable tests by hand. For example "hygiene" on all > glassware has to be perfect as a single finger print can send you off scale. > The machines self clean themselves and as importantly their working fluid. > Get a bigger tank! > > Regards > > Mike > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart > Sent: Thursday, March 01, 2012 11:12 PM > To: [log in to unmask] > Subject: [TN] under-mask cleanliness of large panel > > TechNetters, we have a panel that is too large to fit in the test tank of an > Omegameter. Dimensions, in inches, are 21 x 24. Is there an Omegameter-like > instrument, or another model of Omegameter, that can accommodate such a > large panel? > > One of our people suggested 'washing' the panel, a la the IPC test method > for ROSE, and putting the solution into the Omega meter. How well would that > work? > > Any other ideas? Thanks.... > > Louis Hart > Compunetics > Monroeville, PA > USA > [log in to unmask]<mailto:[log in to unmask]> > 412-858-1232 > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________