Ditto. The HiV boards were never a problem, the oil boxes were. drip-drop-drip-drop....open, clean, reweld, seal...drip-drop.....open, clean, reweld, seal...drip....open, clean, reweld, seal...AAAAAaaaaahh..... Inge PS. only job I know where you worked with one hand in the pocket. On 29 March 2012 16:42, Phil Nutting <[log in to unmask]> wrote: > William, > > Can you be more specific about your needs/troubles? We design and build > many different high voltage boards for our high voltage power supply > products with typical outputs between 160 and 180kV (submerged in oil) and > we have been successful at 40 to 100kV in air. > > > Phil Nutting > Design for Manufacturing Engineer > Kaiser Systems, Inc. > 126 Sohier Road > Beverly, MA 01915 > Phone: 978-922-9300 x1310 > Fax: 978-922-8374 > e-mail: [log in to unmask] > www.kaisersystems.com > www.linkedin.com/in/philnutting > > > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of William Noel > Sent: Tuesday, March 27, 2012 6:10 PM > To: [log in to unmask] > Subject: [TN] Hi Voltage Board Design > > Hello all - Is anyone aware of a good training program that addresses > design of high voltage pcb's? I'm a little out of my comfort zone with > regard to hi-voltage spikes, switching and the subsequent affect on other > areas of the board. Thanks in advance for any advice. > > > Note: All the information contained in this e-mail and its attachments is > proprietary to Kaiser Systems, Inc. and it may not be reproduced without > the prior written permission of sender. If you have received this email in > error, please immediately return it to sender and delete the copy you > received. > > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________