photos would be great -- nooks and crannies are generally problematic in a plated hole -- good vibration is important in electroless -- assuming a standard thickness, your aspect is only 6:1, so no rocket science -- viscosity can also be an issue -- there are additives to reduce surface tension and improve wetting in holes -- but again, for 6:1 this is pretty bread-and-butter plating -- but best to get a nice microsection view -- a little concerned about the nooks etc From: drilbert <[log in to unmask]> To: TechNet E-Mail Forum <[log in to unmask]>, Ian Hanna <[log in to unmask]> Date: 26/03/2012 01:32 PM Subject: Re: [TN] Fw: [TN] plating void Thanks Ian. I will send a picture. The part has certain nooks and crannies where the voids tend to occur. From your input it sounds like bubbles are a common process risk with plating baths that we must pay attention to and manage how to prevent. The vibration in place may need to be reconfigured or replaced. It seems weak. I couldn't feel much vibration translating into the rack. Mark Julstrom From: Ian Hanna <[log in to unmask]> To: [log in to unmask] Sent: Monday, March 26, 2012 6:44 AM Subject: Re: [TN] Fw: [TN] plating void thanks dwight -- yes -- a picture is worth many many words -- mark, the simplest explanation is electroless copper voiding via bubbles -- bubbles are very much a part of the process -- the trick is not to let them collect in the small holes -- vibration helps -- there is a whole science behind that -- rack/bar vibration electric/air -- i once found my (rack) air vibrators in one shop were worn out -- they made lots of noise still, but running a vibrometer, they didn't actually do much anymore -- don't have any numbers tho, just anecdotes now for this. we replaced the worn out units and life was good -- also -- be very careful if you try to do a web-search on this topic...i learned that the hard way also... the good news is that this mode is fairly black and white -- if there is a (full) bubble void, you see it, if there is none it passes -- you won't get half a bubble void... i would want to confirm the root cause just to be safe - but the exposed laminate is a fair indicator From: Dwight Mattix <[log in to unmask]> To: <[log in to unmask]> Date: 23/03/2012 04:42 PM Subject: Re: [TN] Fw: [TN] plating void Sent by: TechNet <[log in to unmask]> Looks like you missed part of what Ian was saying there... Let me try to expand on that: It could have been a) skipped by electroless Cu plating and therefore not electrolytically plated at all. b) If it was first plated fine by electroless and then successfully electrolytic plated. It could then be etched out down to base dielectric if there was skip in the etch resist plating. In either case it would show a bare dielectric in the hole wall. They will have different copper shape leading into the void though depending on source of the missing copper. Once more with feeling: A picture is worth a thousand words. Of a cross-section that is... At 01:18 PM 3/23/2012, [log in to unmask] wrote: >It is a base dielectric material. The plating portion of the wet >process begins with an electroless Cu bath. > > > >----- Forwarded Message ----- >From: Ian Hanna <[log in to unmask]> >To: "[log in to unmask]" <[log in to unmask]> >Sent: Friday, March 23, 2012 12:47 PM >Subject: Re: [TN] plating void > >do you mean base dielectric material, or base copper material -- an >electrolytic copper plating void will still leave the base copper >intact if it is caused by a bubble -- what is the shape of the >edges, is it tapered or rounded -- is the void in the centre of the >hole or towards the outside? any photos? could be electroless copper >void electrolytic copper void tin void dry-film residue >From: "[log in to unmask]" <[log in to unmask]> >To: <[log in to unmask]> >Date: 23/03/2012 03:41 PM >Subject: [TN] plating void >Sent by: TechNet <[log in to unmask]> > >________________________________ >I'm looking for input on the following plating defect. > >I observe a plating void that occurs on a Cu plated feature with >ENIG finish. The void goes down to the base material. The defect >is typically .002 diameter. The feature size is .010 across. The >parts run on a manual plating line and hang on a small plating rack. > >The plating engineer believes the root cause of the void is a bubble >on the part during plating. The action plan includes implementing >stronger vibration on the part in the plating bath. > >I have two questions. >1. How much vibration is typically needed to avoid developing a >bubble on a part during plating? >2. For this plating void defect, is it possible that Ni corrosion >or other reliability concerns would eventually develop if defective >parts escaped? > >Thank you, > >Mark Julstrom > >______________________________________________________________________ >This email has been scanned by the Symantec Email Security.cloud service. >For more information please contact helpdesk at x2960 or [log in to unmask] >______________________________________________________________________ > >______________________________________________________________________ >This email has been scanned by the Symantec Email Security.cloud service. >For more information please contact helpdesk at x2960 or [log in to unmask] >______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________