Fellow TechNetters: Sn-77.3, Cu-0.07 Can someone provide a recommended etchant for the above stated alloy. Want to determine micro structure. Victor, ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________