Rich, you may be thinking of Table A-VI, on page 41 of MIL-PRF-55110 rev G amendment 3. If you don't have the spec, go to http://dodssp.daps.dla.mil/ . I think I've seen it other place(s), too. Louis Hart -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski Sent: Thursday, February 16, 2012 3:00 PM To: [log in to unmask] Subject: [TN] Correlation Factors for ROSE Testing While I realize that IPC specifically and the industry in general, does not support the use of ROSE correlation factors for the various testers, I have a need to see the official document that at one time quoted these specifically allowed factors. I took a cursory look though all 230 pages of IPC TR 583 and didn't see that table. I seem to recall a military specification that had that table. Was it 454? 28809, 2000? Does anyone recall? Rich Kraszewski / PLEXUS ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________