We use Kester 2120 WS halide free flux both as spray and foam application in our wave (tin-lead assembly). It can be thinned with IPA for foam application. We started using this flux about 6 years ago for the same reason for a medical customer of ours. This flux has been easy to clean in our application with straight DI in-line wash (135 F) Regards, Amol Kane Process Engineer AsteelFlash US East Corp Tel: (607) 687.7669 x349 (O) www.asteelflash.com This e-mail and any attachments are confidential. It is intended for the recipient only. If you have received this e-mail in error, please immediately notify the sender by replying to this e-mail and delete the e-mail and all copies from your computer. Although the sender and AsteelFlash have taken every reasonable precaution, the e-mail and attachments may have some errors or omissions and may contain viruses. We cannot accept liability for any damage that you sustain as a result of that. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting Sent: Tuesday, February 28, 2012 2:13 PM To: [log in to unmask] Subject: [TN] halides in water soluble fluxes We have some parts that are sensitive to halides in flux, specifically some thru-hole opto devices. We are currently using a water soluble flux that contains halides. In doing some very quick research it looks like the WS fluxes have halides and the NC fluxes do not. Is there a halide free WS flux for lead-free wave soldering (foam application)? We need the WS fluxes because we currently use a DI water only batch wash system. Washing the boards is mandatory for our applications. Thanks in advance, Phil Nutting Design for Manufacturing Engineer Kaiser Systems, Inc. 126 Sohier Road Beverly, MA 01915 Phone: 978-922-9300 x1310 Fax: 978-922-8374 e-mail: [log in to unmask]<mailto:[log in to unmask]> www.kaisersystems.com<http://www.kaisersystems.com> www.linkedin.com/in/philnutting<http://www.linkedin.com/in/philnutting> ________________________________ Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________