Technetters, we are looking into possible changes in the electroplating process for printed circuit boards. Possible measures for the effect of changes on reliability of internal connections under consideration are the 'Highly Accelerated Thermal Shock' and the 'IST' as in TM-650, 2.6.26. May I have some comments or guidance on the characteristics and merits of these two tests, or any others that we ought to consider? I leave it to your discretion, to determine if an off-line response is preferable than one to TechNet. Louis Hart Compunetics Monroeville, PA USA [log in to unmask]<mailto:[log in to unmask]> 412-858-1232 ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------