We did some experiments with our paste and when correctly stored we have extended the life by 3 months without any discernible problems. You would need to do your own experiments with your paste and the experiment should take into account the target usage. The above is another way of saying 'it depends' but that is someone else's catch phrase. Rex Rex Waygood Technical Manager Hansatech EMS provides value manufacturing through engineering and quality Hansatech EMS Limited Benson Road Nuffield Industrial Estate Poole Dorset BH17 0RY United Kingdom Tel: 01202 338200 Fax: +44 1202 338202 DDI: 01202 338222 [log in to unmask] www.HansatechEMS.com -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Juliano Pacheco Sent: 16 January 2012 13:30 To: [log in to unmask] Subject: [TN] Expired Solder Paste Hi, What are the consequences of using expired solder paste? How long after the expired date is "acceptable"? Thank you. Juliano Pacheco ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------