同意你的看法,因为此焊点连接着一条长条铜线,所以该焊点需要的热量更多。 ----- 原始邮件 ----- 发件人:Lu Chunli <[log in to unmask]> 收件人:<[log in to unmask]> 主题:Re: [TGAsia] 润湿角问题 日期:2011年12月08日 16点55分 应该是炉温的问题,而且是因为两次上锡的原因。第一次的焊点没有完全熔化。 From: Zhaojunbo [mailto:[log in to unmask]] Sent: Thursday, December 08, 2011 4:42 PM To: Asia Committe Task Group Forum; Lu Chunli Subject: 答复: 润湿角问题 什么原因造成的?从图片上看与周边焊点差异较大 This e-mail and its attachments contain confidential information from HUAWEI, which is intended only for the person or entity whose address is listed above. Any use of the information contained herein in any way (including, but not limited to, total or partial disclosure, reproduction, or dissemination) by persons other than the intended recipient(s) is prohibited. If you receive this e-mail in error, please notify the sender by phone or email immediately and delete it! 发件人: TGAsia [mailto:[log in to unmask]] 代表 Lu Chunli 发送时间: 2011年12月8日 14:31 收件人: [log in to unmask] 主题: [TGAsia] 润湿角问题 大家帮我看看这个种焊点应该算做哪种不良,润湿不好?但是又觉得不是缺陷吧?谢谢! Lu Chunli IPC Training Specialist Tel: +86 10 6789.2929 - 190 Mobile: +86 13810570188 Email: [log in to unmask] www.enics.com Important: This email transmission is intended only for the person or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and delete the material from any computer. (C) 2010 Copyright Enics Group. All rights reserved. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ Important: This email transmission is intended only for the person or entity to which it is addressed and may contain confidential and/or privileged material. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. If you received this in error, please contact the sender and delete the material from any computer. (C) 2010 Copyright Enics Group. All rights reserved. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________