用EDS(能譜分析儀)確認它的元素成分,再結合FTIR(傅立葉紅外光譜儀)確認.
From:
TGAsia [mailto:[log in to unmask]] On Behalf Of George
Fu (CARLISLE)
Sent: Friday, November 04, 2011
1:58 PM
To:
Subject: [TGAsia] black dot on the
solder cap
请教各位:
如下连接器来料出现黑色斑点,我们感觉像是氧化,有什么办法知道是否是氧化还是别的?
另外,有关除金的问题,大家是否了解在航空航天产品,除金是否是必须的,我没有J-STD-001ES的标准,所以不知道它的标准
到底是怎么介定的。
有朋友知道吗?
George Fu
Engineering Department
Tel:
(86)-769-83454979 / 977 / 976 ext. 25
Fax:
(86)-769-83454972
__________ Information from ESET NOD32 Antivirus, version of virus signature
database 6599 (20111103) __________
The message was checked by ESET NOD32 Antivirus.
http://www.eset.com
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
*************************************************************************************************************************
This email message, including any attachments, is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply e-mail and destroy all copies of the original message. [Delta Electronics (Jiang Su) Ltd.]
*************************************************************************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________