BGA失效分析只有X-RAY是遠遠不夠的.
切片的設備最起碼要有,最好還要有SEM/EDS等.
From:
TGAsia [mailto:[log in to unmask]] On Behalf Of woaini888
Sent: Tuesday, November 15, 2011
9:50 AM
To:
Subject: Re: [TGAsia] BGA芯片 切片分析
你可以买一台X光机啊专用的啊
在 2011-11-14 15:11:44,fan <[log in to unmask]>
写道:
各位高手:
请教下哪家公司可以对外承接BGA芯片焊接的切片和红墨水分析的?客户要求我们提供这方面的报告。非常感谢!
Best Regards
Fan
Office:86-592-5699313
Fax:86-592-5621095
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
*************************************************************************************************************************
This email message, including any attachments, is for the sole use of the intended recipient(s) and may contain confidential and privileged information. Any unauthorized review, use, disclosure or distribution is prohibited. If you are not the intended recipient, please contact the sender by reply e-mail and destroy all copies of the original message. [Delta Electronics (Jiang Su) Ltd.]
*************************************************************************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________