Yes. Doug said it better than I. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls Sent: Thursday, October 27, 2011 4:12 PM To: [log in to unmask] Subject: Re: [TN] ESD packaging material issue In addition Wayne, if the boards are being put into the bags directly after a heat-based cure (e.g. oven) and you do not allow them to cool to room temperature first, the coating will stick to the bags. Check to see when your operators are putting the assemblies into the bags and make sure they are not shortcutting the cure process. Doug Pauls Phil Bavaro <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 10/27/2011 03:58 PM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to <[log in to unmask]> To <[log in to unmask]> cc Subject Re: [TN] ESD packaging material issue Wayne, Something doesn't sound right here. Solithane S-113 is a polyurethane and my experience is that fully cured urethane does not normally stick to the static dissipative interior of a multilayer ESD shielding bag. I would check to ensure that the conformal coating is fully cured before it gets put into the bag. I'll admit I haven't ever used Solithane S-113 and had a hard time finding the data sheet. Uniroyal was the manufacturer on the only archived datasheet I could find but the current website eluded me. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of E-Mail Forum Wayne Knapp Sent: Thursday, October 27, 2011 1:13 PM To: [log in to unmask] Subject: [TN] ESD packaging material issue Hi Technetters, I could use your help resolving an issue I?m having with the ESD bags that we are currently using for packaging. The ESD bags are sticking to the conformal coating (Solithane S-113) on the CCAs that are placed in the bag. We cannot change the coating that is used on the CCAs, so we are looking for ESD safe packaging bags that will not stick to the CCAs. Does anyone know if there is an ESD bag (material) that would not stick to the CCAs? Any help identifying a suitable ESD bag material and supplier would be appreciated. Thanks, Wayne --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ------------------------------------------------------------------------------ This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------