Yeah, what he said. I know from our past internal studies that we get static electricity generation that are in high levels with things like silicone adhesives or urethane adhesives dispensed as staking compounds. And when you have components that can be damaged by as little as 50 volts, that is a reliability hazard. We have air ionizers going in such applications, along with properly grounded ESD mats and wrist straps for the operators. Inge, there is not enough Diet Mt. Dew in Iowa for me to even try to figure out the physics behind triboelectric charging mechanisms between a liquid insulator and a solid insulator. The issue that we have, which prompted my original question, is that much of our conformal coating is done by hand (don't ask why). The acrylic coating used has a high solvent load with a relatively fast evaporation rate. Besides the pneumatic syringes, we have small open containers of conformal coating. The air ionizers blowing across the coating booth has a tendency to evaporate the solvent, making the coating very stringy and viscous. Leads to a lot of waste. It makes the operators jobs harder. And of course, our managers do not want to incur the cost of putting an air ionizer in every booth. Static dissipative materials would be the preferred route to eliminate the charging in the first place. The operators did not like the black carbon loaded ones that we use because they cannot see how much coating is left in the tube as they can with a translucent body. Some programs re-use syringes, some do not. Static dissipative syringe bodies are expected to be more expensive, so Enterprise Sourcing (or as we call them, The Enemy) will have a conniption fit over increased costs and so some sort of sleeving device would be a desired alternative from their perspective. The last time we looked, our existing vendors wanted very large minimum orders for these and did not really have them as stock items for off the shelf purchase. Which is why I originally went to this forum to see what solutions you guys were using. Still looking for something along the lines of "we use Bob's House O' Syringes, part number BR-549". I do have a call in to Ellsworth Adhesives, one of our suppliers, as was suggested. Doug Pauls "Stadem, Richard D." <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 09/14/2011 08:15 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Stadem, Richard D." <[log in to unmask]> To <[log in to unmask]> cc Subject Re: [TN] Pneumatic Syringes and ESD Okay. Gotta tell you. ESD generation of fluids of all types has always been a major issue in many manufacturing fields, especially in the automotive, boat, metal furniture, etc. epoxy paint applications and very especially the medical profession. So yes, there are dissipative syringes, tips, and special holders that ground the syringe back to the machine's electrical ground. Just so you know, the Navy recently expressed a concern with ESD charges occurring from epoxy application. They reviewed our process, but I only use the dissipative syringes, so no issues. However, I do know that there has been a major push away from the poly syringes to dissipative within the industry. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick Sent: Wednesday, September 14, 2011 6:33 AM To: [log in to unmask] Subject: Re: [TN] Pneumatic Syringes and ESD Inge, I have seen many materials that 'string' like crazy when dispensing - conductives and non-conductives. I've always used localized ionized blowers in situations where stringing is observed, in the belief that 'stringing' was related to charge generation - and for the most part, this has greatly reduced the stringing. While not scientific 'proof' of charge generation, it might support the concept. When the dispensed material's tail separates from the dispense needle, it can take off large distances in any horizontal direction. Some materials seem to throw a string equal in length to the dispense height. Even the conductive paste materials have a large percentage of non-conductive resins involved. Some silicones can be even more messy. Could charge generation be related to a shearing effect as the material is extruded through a needle, or past the brush hairs in Doug's case? Could the repeated time pressure pulse of a dispenser's compress and release of the material within the syringe to the extent that charge generation is taking place within the bulk of the material [on a molecular scale]??? And possibly what I call 'stringing' has nothing to do with charge generation... Personally, I believe that an antistatic syringe barrel and piston is less effective than a well controlled workstation. Even if the barrel and piston are antistatic, are static dissipative needles available? What about the vinyl hose coming from the dispenser to the barrel adapter at the syringe end of the hose? Is that antistatic as well? What about the plastic fitting on the end of the vinyl hose going into the plastic fitting on the face of the dispenser unit? Be interesting to hear comments. Best regards, Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord Sent: Wednesday, September 14, 2011 6:33 AM To: [log in to unmask] Subject: Re: [TN] Pneumatic Syringes and ESD Doug, Triboelectric means adding or stealing electrons through friction. How can a uncured glue (liquid with a high viscosity) move electrons from your nozzle? I've been in the game for decades and not heard about such things. I've participated in p-p courses, glue courses, read lots of articles etc, but missed what you insist. Human and dry hair has a molecular crystal-like surface, and via the Fermi level you can move electrons from the orbit. However, if your hair is fat, there will be no charge movements, because the fat has no specific surface for that purpose. Likewise, I thought uncured glues were no aspirants either. Well, never too late to learn something new. Inge Relationship between *triboelectric* charging and surface *...* < http://search.mywebsearch.com/mywebsearch/redirect.jhtml?qid=62bac059e5f09c b4c1291b201f0024f4&searchfor=kinetic+explanation+of+triboelectric+charges&ac tion=pick&pn=1&n=77decd8b&ptb=naCNCR5Azm75RkmBmXss1w&ptnrS=ZRxdm784YYSE&ss=& st=hp&cb=ZR&pg=GGmain&ord=4&tpr=hpsb&redirect=mPWsrdz9heamc8iHEhldEWVlFOy8LX VdR6PzojpERxbLlEmRQOowS8Qj5BmJGVqQkswtwN%2FH7EAkxVp0REdxDZ8QU9G9gHdhVQrRQ2vn %2FnU%3D&ct=AR> bleaching, and oxidative dyeing has only a small effect on *triboelectric*charging. Measurements of the *kinetics* of *charge* decay indicate that none of these *...* http://journal.scconline.org/pdf/cc1985/cc036n03/p00189-p00212.pdf - Cached< http://search.mywebsearch.com/mywebsearch/redirect.jhtml?redirect=GGc ached.jhtml&action=click&searchfor=kinetic%2Bexplanation%2Bof%2Btriboelectri c%2Bcharges&curl=http%3A%2F%2Fjournal.scconline.org%2Fpdf%2Fcc1985%2Fcc036n0 3%2Fp00189-p00212.pdf&isDirResults=false&tpr=hpsb&cid=KYJrE_TQtsAJ&ptnrS=ZRx dm784YYSE&st=hp&ptb=naCNCR5Azm75RkmBmXss1w&ct=GC&pg=GGmain&n=77decd8b> On 13 September 2011 20:06, Douglas Pauls <[log in to unmask]>wrote: > The coating is insulative in its liquid state as well. > > Doug Pauls > > > > "Mike Fenner" <[log in to unmask]> > 09/13/2011 12:48 PM > Please respond to > <[log in to unmask]> > > > To > "'TechNet E-Mail Forum'" <[log in to unmask]>, <[log in to unmask]> > cc > > Subject > RE: [TN] Pneumatic Syringes and ESD > > > > > > > You would have to check with supplier, or verify it yourself; but though > the > coating is insulating when cured it may well not be uncured in liquid > form. > > Regards > > Mike > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls > Sent: Tuesday, September 13, 2011 4:53 PM > To: [log in to unmask] > Subject: [TN] Pneumatic Syringes and ESD > > Good morning all, > > Time for a silly question. The question has been raised internally as to > the risk of ESD generation when an acrylic conformal coating (an > insulative material) is applied using pneumatic syringes (also an > insulative material), through a nylon brush (a third synthetic material). > > 1. Do you know of any studies done benchmarking static generation levels? > > We have done some here, but want to do a sanity check. > 2. If you have such devices in your facilities, what are your mitigation > efforts? Air ionizers, grounded tubes? > 3. Does anyone use, and can recommend, ESD safe syringe bodies and caps? > > Many thanks in advance. > > Doug Pauls > Rockwell Collins > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 16.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > For additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > > > > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 16.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > For additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------