Hi Jim - Our board fabricators do a great job so I have never asked the question. Our typical via is in the 8 mil to 13.5 mil range and there has been no issue with fill and cap. Our typical board thickness is 63 mil to 100 mils so you can calculate the aspect ratio of a "typical" situation but we should have some Technet board fabricators that can provide a much better answer than I on fill and cap process capabilities. Dave "Marsico, James - ES" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 09/01/2011 07:00 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Marsico, James - ES" <[log in to unmask]> To <[log in to unmask]> cc Subject Re: [TN] QFN with solder slug - plating vias shut Just out of curiosity, what is the rule of thumb for via size for plating vias shut? Does aspect ratio come into play? Jim Marsico ITT Corporation 1500 New Horizons Blvd. North Amityville, NY 11701 631-630-5079 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman Sent: Thursday, September 01, 2011 7:55 AM To: [log in to unmask] Subject: Re: [TN] QFN with solder slug Hi Mark - our preferred method is to plate them shut so that we have no possible issues for either solder thieving or some type of process fluids (either fabrication or assembly) entrapment. The cost of the board increases but we feel the increase is worth it in terms of issue avoidance. Dave Mark Larson <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 08/31/2011 04:21 PM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Mark Larson <[log in to unmask]> To <[log in to unmask]> cc Subject Re: [TN] QFN with solder slug Thanks, I wanted to hear how others are doing it, only thing different we are doing is using 10 mil via, and that should be less of a problem than 12, and we are not connecting all layers to the vias, just the back side. Dave - yes, that is the main point we are now debating, to cap the vias or not with soldermask. By cap I mean put a layer of soldermask just slightly bigger than via hole, then the "normal" layer of solder mask, to the bottom side only of course. as for filling them, we really want to avoid that. Perhaps our real problem is being too conservative (small via, we are only using 5 where the design engineers estimate is 6-8, and not connecting inner same net planes) will prevent enough heat transfer, the whole point of the slug, right? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------