Hi Mark - our preferred method is to plate them shut so that we have no possible issues for either solder thieving or some type of process fluids (either fabrication or assembly) entrapment. The cost of the board increases but we feel the increase is worth it in terms of issue avoidance. Dave Mark Larson <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 08/31/2011 04:21 PM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Mark Larson <[log in to unmask]> To <[log in to unmask]> cc Subject Re: [TN] QFN with solder slug Thanks, I wanted to hear how others are doing it, only thing different we are doing is using 10 mil via, and that should be less of a problem than 12, and we are not connecting all layers to the vias, just the back side. Dave - yes, that is the main point we are now debating, to cap the vias or not with soldermask. By cap I mean put a layer of soldermask just slightly bigger than via hole, then the "normal" layer of solder mask, to the bottom side only of course. as for filling them, we really want to avoid that. Perhaps our real problem is being too conservative (small via, we are only using 5 where the design engineers estimate is 6-8, and not connecting inner same net planes) will prevent enough heat transfer, the whole point of the slug, right? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------