Hi Phil, Depending on what elements you want/need to monitor, you might be able to use XRF (but you'd have to run statistically sound number of measurements). Vladimir SENTEC Testing Laboratory Inc. 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca -----Original Message----- From: Phil Bavaro <[log in to unmask]> Sender: TechNet <[log in to unmask]> Date: Tue, 6 Sep 2011 16:10:30 To: <[log in to unmask]> Reply-To: TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask] Subject: [TN] Solder bath purity testing questions I just installed a small selective solder rework system and now have to start testing the solder bath for purity. Who do you use for testing your solder bath for purity? I cannot seem to find the old standby sources I had used in the past. Do I have to keep the solder purity analysis going back to the same company that I buy the bars from (alp___ to alp___, kes___ to kes___, etc) or has this service been farmed out permanently to independent labs? I am not able to find it quickly on the internet. I thought about trying to use an XRF machine to perform my analysis myself but I am a little skeptical about its' precision. Lastly, I find that the words in J-STD-001 seem a bit excessive for my situation: "Records containing the results of all analyses and solder bath usage (e.g., total time in use, amount of replacement solder, or area throughput) shall be maintained for a minimum of one year for each process/system." Do I really need to record the time that we have the solder molten? I can understand recording volume of solder introduced, but this is a rework pot and the usage and throughput would be minimal. Any help is appreciated. ------------------------------------------------------------------------------ This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------