What went wrong with it. We have repaired our many time over the past 20+ years. We also have a Buehler ISOMET 1000. Great assets of equipment. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart Sent: Tuesday, August 23, 2011 6:29 PM To: [log in to unmask] Subject: [TN] low-speed saw? TechNetters, does anyone have or know where I might find a low-speed saw for sectioning things like ceramic IC packages or PWBs containing ceramic fillers? We had a Buehler ISOmet low-speed, but after many years it failed and cannot be repaired. Contact me off-line if you wish. Louis Hart Compunetics Monroeville, PA USA [log in to unmask]<mailto:[log in to unmask]> 412-858-1272 ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------