Try bidservice.com object # 87 /Inge On 24 August 2011 01:29, Louis Hart <[log in to unmask]> wrote: > TechNetters, does anyone have or know where I might find a low-speed saw > for sectioning things like ceramic IC packages or PWBs containing ceramic > fillers? We had a Buehler ISOmet low-speed, but after many years it failed > and cannot be repaired. Contact me off-line if you wish. > > Louis Hart > Compunetics > Monroeville, PA > USA > [log in to unmask]<mailto:[log in to unmask]> > 412-858-1272 > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 16.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > For additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------