Check the stencil alloy, etching process and stencil frame. The etching area and depth also important parameters. Reuven נשלח מה-iPhone שלי ב-13 ביול 2011, בשעה 17:41, "Gumpert, Ben" <[log in to unmask]> כתב/ה: > Technetters, > > Is there a rule of thumb regarding the amount of step that can be etched into a stencil? > > I've used stencils with 1 and 2 mil steps successfully, but recently I've seen a problem with a 3 mil step (8 mil foil stepped down over most of the printed area to a 5 mil thickness). > > The problem I'm seeing is that the stencil tends to warp around apertures, particularly in areas like fine pitch QFPs, where there are long apertures close together, and the remaining material is a thin strip. This warp makes the stencil act thicker and allow more paste to be deposited, leading to bridges in the fine pitch QFPs. > Anyone seen this problem before? > > Thanks in advance, > Ben > > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 16.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------