Hi Julie, Can you take a picture on the section between the BGA ball and it (component) substrate AFTER you had physically separated them. Did you performed a dye and pry which will show that the contact is "opened" or near "open". Regards GA Tan ________________________________ From: TechNet on behalf of vladimir Igoshev Sent: Fri 7/1/2011 9:28 PM To: [log in to unmask] Subject: Re: [TN] BGA ball dewet from substrate I don't see the details I'd need but it could be caused by spalling at the UBM. Vladimir SENTEC Testing Laboratory Inc. 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca -----Original Message----- From: Steve Gregory <[log in to unmask]> Sender: TechNet <[log in to unmask]> Date: Fri, 1 Jul 2011 07:58:48 To: <[log in to unmask]> Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]> Subject: Re: [TN] BGA ball dewet from substrate Good Morning Julie, I have your picture posted here: http://stevezeva.homestead.com/Solder_dewet.jpg That is pretty strange. I have never seen something like that! Steve -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Thursday, June 30, 2011 8:47 PM To: [log in to unmask] Cc: [log in to unmask] Subject: RE: [TN] BGA ball dewet from substrate Thank you! Here it is, Steve. -------------------------------- Julie Silk Environmental Compliance Technical Program Manager Agilent Technologies 707-577-4296 [log in to unmask] -----Original Message----- From: Wenger, George M. [mailto:[log in to unmask]] Sent: Thursday, June 30, 2011 5:34 PM To: TechNet E-Mail Forum; SILK,JULIE (A-Sonoma,ex1) Cc: Steve Gregory Subject: RE: [TN] BGA ball dewet from substrate Julie, You can send your photograph to Steve Gregory who I've copied and he can post it on his site that is available to all the IPC TN members Regards, George George M. Wenger Senior Principal Reliability / FMA Engineer Andrew Corporation - Wireless Network Solutions 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 Office (732) 309-8964 Mobile E-mail: [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Julie Silk Sent: Thursday, June 30, 2011 6:29 PM To: [log in to unmask] Subject: Re: [TN] BGA ball dewet from substrate The substrate pad shows an intermetallic layer, demonstrating that there had been a metallurgical bond. Also, the surface of both pad and ball are smooth -- not a fracture, but as if reflowed. I have a good picture from the FA report to share once I figure out how. I believe that if you were to analyze the very first layer on the BGA substrate pad, it would have a layer of solder. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------