Could you advise the root casue of this issue and share with us . And pls also provide the acceptable standard for this defect .Many thanks ! -----Original Message----- From: [log in to unmask] [mailto:[log in to unmask]] Sent: Thursday, June 30, 2011 4:07 PM To: Asia Committe Task Group Forum; wuhao Cc: [log in to unmask] Subject: 答复: Re: [TGAsia] PCB 黑焊盘--- 如何对已出现问题的PCB 做相应处理 此现象非黑盘,但的确属于电镀质量问题。 在无铅焊接工艺中比较多见,此问题难通过工艺措施彻底消除。如果采用的是PTH 孔,一般可以接受,连接的可靠性不会有很大问题。 wuhao <[log in to unmask] OM.HK> 收件人 发件人: <[log in to unmask]> TGAsia 抄送 <[log in to unmask] g> 主题 Re: [TGAsia] PCB 黑焊盘--- 如何对已出 现问题的PCB 做相应处理 2011-06-30 15:08 请答复 给 Asia Committe Task Group Forum <[log in to unmask] G>; 请答复 给 wuhao <[log in to unmask] OM.HK> Hi Jutin : Noted . I am checking with the vendor for this case ,but our prouduction line can't not operate normally now ,so i want to ask you for a good solve method. Besides ,could you advise some related temperature profile for this issue of 黑焊盘 . Best regards, HAO IQC Dept. In-Tech Electronics Ltd. 2 Qihang Industrial Park Haoxiang Road, Shajing,Baoan, Shenzhen,P.R,China Tel : +86 755 33262633 From: Justin Wu [mailto:[log in to unmask]] Sent: Thursday, June 30, 2011 2:50 PM To: 'Asia Committe Task Group Forum'; 'wuhao' Subject: RE: [TGAsia] PCB 黑焊盘--- 如何对已出现问题的PCB 做相应处理 Hi Hao, Maybe you can check with your PCB supplier for solve and review your SMT oven temperature profile. Thanks and best regards, Justin Wu Utilux South China Ltd Phone: +86-755-2850 7521 Fax: +86-755-2850 0927 E-mail Address: [log in to unmask] From: TGAsia [mailto:[log in to unmask]] On Behalf Of wuhao Sent: Thursday, June 30, 2011 2:13 PM To: [log in to unmask] Subject: Re: [TGAsia] PCB 黑焊盘--- 如何对已出现问题的PCB 做相应处理 Dear all : 请教大家! 请问已经出现了黑焊盘的PCB ,怎么处理比较好;也就是说,在焊接前针对已有问题的 PCB ,我们怎么处理能减少这种黑焊盘问题的出现呢? (Embedded image moved to file: pic17086.jpg) (Embedded image moved to file: pic02468.jpg) Best regards, HAO IQC Dept. In-Tech Electronics Ltd. 2 Qihang Industrial Park Haoxiang Road, Shajing,Baoan, Shenzhen,P.R,China Tel : +86 755 33262633 CONFIDENTIAL NOTE: The information contained in this email is intended only for the use of the individual or entity named above and may contain information that is privileged, confidential and/or exempt from disclosure under applicable law. If the reader of this message is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete the email. Thank you. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ __________ Information from ESET NOD32 Antivirus, version of virus signature database 6251 (20110630) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com __________ Information from ESET NOD32 Antivirus, version of virus signature database 6251 (20110630) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com __________ Information from ESET NOD32 Antivirus, version of virus signature database 6251 (20110630) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ -------------------------------------------------------- ZTE Information Security Notice: The information contained in this mail is solely property of the sender's organization. This mail communication is confidential. Recipients named above are obligated to maintain secrecy and are not permitted to disclose the contents of this communication to others. This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please notify the originator of the message. Any views expressed in this message are those of the individual sender. This message has been scanned for viruses and Spam by ZTE Anti-Spam system. CONFIDENTIAL NOTE: The information contained in this email is intended only for the use of the individual or entity named above and may contain information that is privileged, confidential and/or exempt from disclosure under applicable law. If the reader of this message is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete the email. Thank you. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________