Jack, We have done exactly that due to the shrinkage of the hard overcoat during curing. Phil Nutting -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson Sent: Wednesday, June 29, 2011 12:16 PM To: [log in to unmask] Subject: Re: [TN] Potting over Conformal Coat? profound thoughts, sensei... (thanks) Another colleague here speculated that the type of potting compound being used was so "hard" that the conformal coat provided a buffer zone for thermal cycling. That was a new concept to me, this is an older product. onward thru the fog, Jack . On Wed, Jun 29, 2011 at 10:59 AM, <[log in to unmask]> wrote: > > Jack you ask a very broad question. I shall use my stock answer of "It > Depends". > > Conformal coating can be applied prior to conformal coating, but you have > to ask why. Usually your potting material provides your environmental > protection. Conformal coating is then non-value added. If it is there to > protect your assembly from the potting material, you probably have the wrong > potting material chosen. > > Are there constituents in potting compounds that can affect components? > Sure. There are lots of compounds out there. Choose wisely. > > Are there residues that can inhibit potting cure? Absolutely. Clean > carefully. Test thoroughly. Choose wisely. > > I feel like the Knight in Indiana Jones and the Last Crusade.... > > Doug Pauls > > > *Jack Olson <[log in to unmask]>* > Sent by: TechNet <[log in to unmask]> > > 06/29/2011 10:39 AM > Please respond to > TechNet E-Mail Forum <[log in to unmask]>; Please respond to > Jack Olson <[log in to unmask]> > > To > <[log in to unmask]> > cc > Subject > [TN] Potting over Conformal Coat? > > > > > Are any of you familiar with conformal coating assemblies before applying > potting compound? > > Are there potting compounds that contain harsh chemicals that could affect > components? > or > Are there residues on boards that can affect the curing properties of > potting compounds? > > I can only find one vague sentence about this in the Working Draft of > IPC-HDBK-850 > (3.12.9.1 Compatibility) > > thanks, > Jack > > > > ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------