We've used the Malcom solder paste spinner units for years with great results. We have two, one for jars and the other for tubes. They're pricey but reliable, and perform according to their ads. They both mix the paste and bring it to room temperature within 10 minutes. http://www.malcomtech.com/Electronics/products_sps.html Never tried the hot dog rollers, but that's thinking outside the box! Leland -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Tuesday, June 21, 2011 9:01 AM To: [log in to unmask] Subject: Re: [TN] Solderpaste Storage and Use LOL. Hi, Dave. Good to hear from you. I totally agree with you. I only purchase paste in tubes, whether the larger Semco tubes (500 or 600 gram size) or the smaller 50cc cartridges that are now available. The jars just don't cut it. In fact, I have found the jars without the inner sealer, the plastic disk that is used to keep moisture out. When I asked what happened to it, one operator told me she throws them out because they get contaminated with paste! She stated it "does a grody on my nail job". You can just imagine my sympathy. However folks, keep in mind that the paste will separate inside the tube over time to some extent. Not sure how the hot dog rollers will work inside the refrigerator. I really think that the centrifuge is a good idea. Probably pays for itself within a year in reduced print defects. From: [log in to unmask] [mailto:[log in to unmask]] Sent: Tuesday, June 21, 2011 7:32 AM To: TechNet E-Mail Forum; Stadem, Richard D. Cc: [log in to unmask] Subject: Re: [TN] Solderpaste Storage and Use Hi Richard - good discussion and information! One comment to add - one of the advantages of we have with solderpaste shelf/use life today that we didn't have back when Doug rode his Mammoth to work is today's modern packaging. The SEMCO tubes only expose the solderpaste to surrounding environment conditions at its ends - a drastic contrast to opening up a jar of solderpaste. And the folks who are using the sealed cartridges also have excellent isolation. Not exposing the solder paste to the surrounding environment any more than necessary for use has been a key parameter in storage/use time. Dave Hillman Rockwell Collins [log in to unmask] "Stadem, Richard D." <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 06/20/2011 04:48 PM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Stadem, Richard D." <[log in to unmask]> To <[log in to unmask]> cc Subject Re: [TN] Solderpaste Storage and Use Please note that solder paste re-certification after shelf life expiration IS allowed, and the methods are listed in the solder paste standard (J-STD-005), including the test methods from IPC-TM-650 and the forms to be used for re-certification. I have done it several times on many different types of paste and different brands, for multiple client companies. I have performed a combination of viscosity tests, printing tests including tact time and open stencil life, and monitored the DPMO of the product that expired lots were used on. The particle size, flux type, leaded or non-leaded alloy did not make any difference. The only thing that mattered (affected the outcome of the test) is the amount of flux separation that occurred while the paste was in storage, and I only found this to be an issue on ONE major brand of paste (don't ask, I won't tell). However, even that paste had zero shift in comparison to the controlled samples when properly mixed. Not surprisingly, expired paste up to 6 months past expiration that had been properly refrigerated throughout its entire 12-month storage life showed absolutely no difference from paste that had been stored and tested exactly the same way BEFORE it expired at 6 months. The six sigma test showed a 99% level of confidence there was no difference in defect data. (P-value test) What was really surprising was the overall DPMO. The number of solder paste defects as seen during the paste print inspection actually improved when expired paste was used! Also, the number of solder joint defects seen after reflow also improved! This was done using surreptitious testing to avoid any Hawthorne effect from the inspectors and operators. All pastes used are now mixed in an automatic centrifuge made for that purpose and the viscosity tested. This eliminates the "sitting at room temperature for 8 hours" and assures the viscosity is good from the start. The right centrifuge (and the right settings) will provide the exact same viscosity and paste temperature every single time a tube is removed from the fridge, once you have established what that mix time is. So, for certain part numbers of solder paste from certain companies, I recommended that the shelf life be permanently extended to 1 year, with no re-certification requirement after the original 6-month shelf life is expired. Remember, this was based on data from repeated testing of several lots over time, and the resulting data was carefully reviewed by both the client company and its customers. It took a little time to develop that database, but it has paid off several times over when smaller EMS companies needed to purchase larger lots of paste than they could use within the shelf life (most distributors require a minimum buy of 20 tubes or so). A single lot of RMA paste "failed" (displayed much worse test results than other candidates during evaluation), but it failed from both the lot sample not yet expired, and the lot sample that was 8 months old and opened for the first time. The reason why? It was shipped from the manufacturer in July, was not kept refrigerated during storage at the distributor, and as it turns out, the paste manufacturer re-marked the lot expiration date. How do I know? Because when I went to pick it up from the distributor, they had ALL of their inventory stored on a shelf at room temp, and when I inspected the paste I found the same C of C used on two different lots with the same date of manufacture, but different expiration dates! Another lot of RMA paste failed because it was shipped frozen in dry ice; that is the worst thing you can do to an RMA paste. So, if you really want to fix your solder paste handling issues, you need to control the paste from the manufacturer, certify only distributors you can audit periodically, and make sure your purchasing requirements detail the proper handling, storage, and shipping methods up to and including the dock door (paste should be removed from the insulated container and placed into the refrigerator within one or two hours from receipt). You absolutely must have some type of internal documentation, training, and auditing system to ensure the paste is stored and controlled correctly once received. Please don't use expired paste based on what I just told you. You need to ensure you have all of the qualification done to validate YOUR particular purchasing, storage, and handling methods for your particular paste. It takes very little time, but once done, it pays off over and over. Does this all seem like a bit of overkill to you? No problem; never mind then, just go back out and support the factory doing all that solder touchup. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner Sent: Monday, June 20, 2011 2:26 PM To: [log in to unmask] Subject: Re: [TN] Solderpaste Storage and Use Hi, I do wonder where all these shelf live ideas comes from. Seems to me that particle size and flux type will make a BIG difference, like a power of 10 or so. A no clean type 3 paste with low levels of activity would seem (at least to me) to last MUCH longer than say type 5 in an active OA flux. Has anyone ever done reflow studies for different types of old paste? I don't think a paste manufacturer would do such a test, I expect to get blasted for even suggesting the idea. But, Look at this link: http://www.endtimesreport.com/Prescription_longevity.html Bob K. Hmmm, I have a bucket of ancient paste tubes. I should give them a try. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Roger Mack Sent: Monday, June 20, 2011 3:12 PM To: [log in to unmask] Subject: Re: [TN] Solderpaste Storage and Use Most pastes have a refrigeration spec. which gives it a shelf life of 6 months. If you are using 600g tubes most datasheets will require 8 hours to acclimatise. Once out of the fridge we don't return it either, but always sign initials, date and time on each tube. Create an out of fridge "on deck" storage for 3 or 4 tubes, or a daily amount for a line. We use a fixture that fills from the top and you pull tubes from the bottom like a canned drink dispenser. If you take one, add a new one to the top from the fridge. You will never run into trouble with your acclimitizing time, or pull too much. Your paste likely has a shelf life for room temperature, so set a spec. that discards all open tubes when pulled, for say, two weeks or a month. If you are using jars and storing working paste, sign and date it as well and control the out of fridge time for that as well. Roger Mack P.Eng. Manufacturing Specialist Parker Hannifin Canada Electronic Controls Division 1305 Clarence Avenue Winnipeg, MB R3T 1T4 Canada direct 204 453 3339 x373 [log in to unmask] www.parker.com/ecd From: Amol Kane <[log in to unmask]> To: <[log in to unmask]> Date: 06-20-2011 13:27 Subject: [TN] Solderpaste Storage and Use Sent by: TechNet <[log in to unmask]> I am re-writing our solderpaste use and storage procedures for water soluble and no clean fluxes (SnPb and Lead-free) to say, in essence the following: "To be stored per the manufacturer's recommendations (usually upto 10C), must be at room temperature before it is dispensed on the stencil (at least an hour thawing is required). Maximum use period to be 8 hours. Re-refrigeration and use beyond 8 hours not permitted" The pushback is to the prohibition of re-refrigeration (for use the next day) after it is thawed and use beyond 8 hours requirement. These requirements are due to concerns with moisture absorption by the solderpaste once thawed (affecting slump) and flux activity (due to ageing) What criteria are all the learned folks on technet using for solderpaste management? Is there any literature available that looks at solderpaste use limits on time and temperature? A logical solution would be to do a DOE to look at these parameters, but I am being asked to come up with something ASAP:). love how these things work! Thanks in advance Amol ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- "PLEASE NOTE: The preceding information may be confidential or privileged. It only should be used or disseminated for the purpose of conducting business with Parker. If you are not an intended recipient, please notify the sender by replying to this message and then delete the information from your system. Thank you for your cooperation." ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------