ROCKY 提到的应该是焊接后产品焊脚结合力的的推力测试吧? 跟应力测试有区别! 发件人: TGAsia [mailto:[log in to unmask]] 代表 Justin Wu 发送时间: 2011年5月20日 10:04 收件人: [log in to unmask] 主题: Re: [TGAsia] 回流炉中焊接的应力测试 可否追溯到相关标准? Thanks and best regards, Justin Wu Utilux South China Ltd Phone: +86-755-2850 7521 Fax: +86-755-2850 0927 E-mail Address: [log in to unmask] _____ From: TGAsia [mailto:[log in to unmask]] On Behalf Of Rocky Wang Sent: Friday, May 20, 2011 9:32 AM To: [log in to unmask] Subject: Re: [TGAsia] 回流炉中焊接的应力测试 1 0201C 1.2KGF 2 0201R 1.5KGF 3 0402C 1.5KGF 4 0402R 1.8KGF 5 0603C 2.0KGF 6 0603R 2.2KGF 7 0805C 2.2KGF 8 0805R 2.5KGF 9 1206C 2.8KGF 10 1206R 3.0KGF 11 1206 以上阻容元件>3.0KGF 12 MEIF SOF IC ( 8pin ) 3.5KGF 13 IC ( 8pin以上) 4.0KGF 14 SOT 23 2.8KGF 15 SOT 14 3.0KGF 柔性板 1 0201C 1.5KGF 2 0201R 1.8KGF 3 0402C 2.0KGF 4 0402R 2.2KGF 5 0603C 2.5KGF 6 其余零件均需>2.8KGF。 推力测试条件: 1. 推力計与PCB面呈45度。 2. 从元件宽的一面推。 3. 冷却后测试 Best Regards Rocky From: TGAsia [mailto:[log in to unmask]] On Behalf Of Peng Yunjun Sent: Thursday, May 19, 2011 9:44 AM To: [log in to unmask] Subject: [TGAsia] 回流炉中焊接的应力测试 各位老师大家好, 谁有回流炉中焊接应力的测试方法? 谢谢分享。 Peng Yunjun(Mr) 彭云军(先生) CACC PT Department [log in to unmask] +86-431-84684785 13756139127 ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ __________ Information from ESET NOD32 Antivirus, version of virus signature database 6136 (20110519) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com __________ Information from ESET NOD32 Antivirus, version of virus signature database 6136 (20110519) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com __________ Information from ESET NOD32 Antivirus, version of virus signature database 6136 (20110519) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________