AI后再SMT,因为红胶是點膠机點的.基本AI不會走锡膏制程.不知其它前輩家怎么做的.能否分享?
 

Thanks&Best Regards!
QE/sharp_zhang(張鵬宇)
Tel:0769-87915950 Ext:
36323
E-mail:[log in to unmask]

-----Original Message-----
From: TGAsia [mailto:[log in to unmask]]On Behalf Of Jessy Lai
Sent: Tuesday, May 03, 2011 10:37 AM
To: [log in to unmask]
Subject: [TGAsia] 答复: [TGAsia] SMT?网厂家

 对于AISMT的先后,以我的经验来说,是先SMT后再AI,因为如果AI后再SMT,怎么印锡膏或红胶?

 对于SMT后再AI会掉件,主要发生在红胶网,则需考虑红胶量,根据不同元件大小

决定开孔。

 

Thanks & Best Regards,

 PE  Jessy.Lai

**************************************

Telephone : +86-0769-872909918829

No.6 Lindong 3Road Lin Cun Industral Center

TangXia Dongguan Guangdong,P.R.C

Email : [log in to unmask]

Website : www.note.se

 

发件人: TGAsia [mailto:[log in to unmask]] 代表 David Lau
发送时间: 201153 10:26
收件人: [log in to unmask]
主题: Re: [TGAsia] SMT钢网厂家

 

确实是这样的。

 

Regards!

David Lau | Assistant Manager - Telecom PIE | Embedded Computing & Power | Fuyong

Emerson Network Power | Emerson Industrial Park, Feng Tang Road, Fuyong Bao'an District | Shenzhen City 518103 China
T
+0755 2961 6219 | F +0755 2961 6499

www.Emerson.com/EmbeddedComputing
| www.Emerson.com/EmbeddedPower Connect with Embedded Computing & Power on Facebook, Twitter and YouTube.

 

From: TGAsia [mailto:[log in to unmask]] On Behalf Of 郑立鹤
Sent: 2011
53 10:17
To: [log in to unmask]
Subject: [TGAsia]
答复: Re:[TGAsia] SMT钢网厂家

 

谢谢!

在上周外出审核钢网供应商时了解到一个情况,向大家了解一下,

就我们以前的经验,如果产品需要进行AISMT(红胶工艺),通

常是先AI后,再用铜网或胶网刷胶。但也有公司会先SMT后再AI

通常我们认为如果采用第二种方式可能会导致掉件和元件损伤。

请问是这样的吗。有没有谁有这方面的经验。

谢谢!

郑立鹤


发件人: wubosz [mailto:[log in to unmask]]
发送时间: 2011429 20:21
收件人: Asia Committe Task Group Forum; 郑立鹤
主题: Re:[TGAsia] SMT钢网厂家

 

您好!

     很少有钢网checklistIntel公司审核过允升吉钢网厂家。但是没有见过intelchecklist。个人经验:

1)激光切割机的定位精度。

2)钢网开口尺寸的一致性。

3)钢网开口的位置精度。

4)孔壁粗糙度。

--

吴波

[log in to unmask]

13602585865


2011-04-28 17:13:08"郑立鹤" <[log in to unmask]> 写道:

各位前辈,大家好!

      请问谁有SMT钢网厂家的审核经验,如何在设备,人员,生产流程

等方面去衡量厂家的实力,有没有相关的checklist可供参考。

 

谢谢!!!

2011-04-28

电子工程郑立鹤

伊戈尔电气股份有限公司

佛山市南海区简平路桂城科技园A3

MP18666577208      zip code:528200

Tel0757-86256771

E-mail[log in to unmask]

Websitewww.eaglerise.com 

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

 


体验网易邮箱2G超大附件,轻松发优质大电影、大照片,提速3倍!


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________