or if it is on print -- military qualification, for example, requires separate qualification for foil lamination...it's an anachronism, but you are contractually bound just the same -- Ian From: Harris Dy <[log in to unmask]> To: <[log in to unmask]> Date: 17/05/2011 05:09 PM Subject: Re: [TN] Core vs Foil Lamination Sent by: TechNet <[log in to unmask]> Absolutely! After mass lamination, you won't even recognize if the panel that came out of the press was foil laminated or core laminated. Foil lamination is now the more popular way of building multilayer boards. The only reason you would want to do core lamination is if the design involves sequential lamination or blind/buried via technology. Thanks, Harris --- On Tue, 5/17/11, Marsico, James - ES <[log in to unmask]> wrote: From: Marsico, James - ES <[log in to unmask]> Subject: [TN] Core vs Foil Lamination To: [log in to unmask] Date: Tuesday, May 17, 2011, 10:39 AM Good Day Technet: We have a heritage PWB design for a space application where our drawing requires a core laminating process. One of our suppliers is requesting using foil lamination in lieu of core lamination for registration issues. Since we qualified the original core lamination, can foil lamination be a direct substitute? Thanks in advance, Jim Marsico ITT Corporation 1500 New Horizons Blvd. North Amityville, NY 11701 631-630-5079 [log in to unmask]<mailto:[log in to unmask]> ________________________________ This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------