建议烙铁头使用刀型烙铁头,温度不超过420度,时间不宜过长,烙铁可选用功率较大的。 Best regards Tom Zhang (张涛) Customer Service Department FIC (Suzhou) Inc. Tel: +86 512 62581988 Ext:5629 Fax:+86 512 62581973 Email:[log in to unmask] ________________________________ 寄件者: TGAsia [mailto:[log in to unmask]] 代理 Jerry Li 寄件日期: 2011年4月11日 11:23 收件者: [log in to unmask] 主旨: [TGAsia] 请教 大家好,请教个问题:排插多引脚连接器相邻引脚(多层板、大焊盘),波峰焊后两个或多个引脚桥接,80w Weller/HAKKO烙铁温度调至450度,焊接时间较长(10-20m),但有时仍不能移除焊料、维修焊点。请问烙铁温度调至450度焊接风险如何评估?是否有推荐可使用的焊接工具、解决办法、合适温度? 谢谢! Jerry ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________