请参见IPC-A-610E里10.2.7 里面对分板有对缺口和铣切边的减少有定义,对突出部分自己定义,不影响组装为主兼考虑外观。 From: TGAsia [mailto:[log in to unmask]] On Behalf Of Lei Shi Sent: Tuesday, April 26, 2011 8:26 AM To: [log in to unmask] Subject: [TGAsia] 关于PCBA割板是否有IPC定义验收标准 各位好: 有个问题想请教一下大家,不知道大家是否知道有IPC标准定义了PCBA割板以后的要求,我看了一下610E并没有明确定义这个方面的验收要求,是否只要不影响PCBA在后期的装配工作就没有问题了吗??谢谢! Best Regards, Shi Lei Process Quality Engineering, Celestica #448 SuHong Middle Road Suzhou Industry Park,215021 Tel:+86 512 62588111-3602 or 13372147203 email:[log in to unmask] Solid Partners. Flexible Solutions. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please visit http://www.messagelabs.com/email ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________