Hi Raye - Here is a link to John Maxwell's paper - Cracks: The Hidden Defect - on root causes of cracked capacitors. It is one of the best treatments of how our soldering processes can cause cracked capacitors and should be required reading for all new engineers. http://www.avx.com/docs/techinfo/cracks.pdf We have found that visual inspection and/ or thermal cycling will not provide the level of detection that you are looking for. We have subjected suspect capacitors/assemblies to high temp/high humidity (85C/85%RH) and then conducting electrical testing producing better predictive results. That conditioning sequence isn't fool proof but worked better for us in finding damage capacitors. Good Luck. Dave Hillman Rockwell Collins [log in to unmask] "Rivera, Raye" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 04/08/2011 09:55 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Rivera, Raye" <[log in to unmask]> To <[log in to unmask]> cc Subject [TN] Cracked ceramic capacitors Hello Technetters, We had an issue with cracked SMT ceramic capacitors causing boards to fail functional test. We isolated the problem to a reel of parts that contained some cracked caps and purged these. Problem solved. My question is about what to do with boards built with these capacitors before we purged. The boards pass functional test. The concern is that a cracked cap was loaded, but has not yet failed. The range of actions proposed here are: - Temperature cycle the boards between -5 C and 55 C a few times. The theory is that this will flush out any latent defects. - Visually inspect for defects. - Manually change out all the suspect caps, about 50 per board. Does anyone have thoughts on what would be the best method or another idea? We don't have ICT capability. Thanks! Raye Rivera ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------