Dear : you can refer to IPC-TM-650 2.4.1, 2.4.28.1 test. Many Thanks, Best Regards, Zhao Zi De QA Department World Mastery Technology Limited Tel:+86 769 85569149 Ext:862 Fax:+86 769 85262272 Email:[log in to unmask] ----- Original Message ----- From: Owen Zhou To: [log in to unmask] Sent: Wednesday, March 16, 2011 1:30 PM Subject: [TGAsia] PCB板绿油的表面附着力 Hi, all: 下午好! 请问PCB板绿层的表面附着力的测试方法应采用什么标准? 其附着力的标准是多少? 谢谢! Owen Zhou ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________