http://ww1.microchip.com/downloads/en/DeviceDoc/21178G.pdf I looked up the package and print info, but cannot see anything that would lead me to think it was a vendor issue. I think Brian Ellis nailed it, it is probably some type of flux inhalation during the tinning of the part. You should see if you can buy a handful of parts direct from the vendor with no tinning done and verify that is what it is. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis Sent: Tuesday, March 15, 2011 10:28 AM To: [log in to unmask] Subject: Re: [TN] Posting cleaning question for IPC user Difficult to say. Firstly, what kind of IC? I suggest à priori that the product may be a heavy polyglycol, without being categorical. Some ICs, especially epoxy DILs and possibly SOICs, were tinned using activated polyglycol-based fluxes and they were notorious for the flux penetrating under a poorly adherent epoxy/lead "joint". I have seen ICs with 0.2-0.3 mm gaps between the lead and the epoxy, ideal capillaries for flux residues. Note that I'm not saying that this is the cause in Jean-François' case, but it does spring to mind. Brian On 15/03/2011 16:48, Jack Crawford wrote: > As Jean-Francois notes, his company policy doesn't permit him to subscribe to technet. If anyone has any suggestions or ideas, please also send your comments to him when you reply to TechNet. > > Thanks > Jack Crawford > IPC > > From: Jean-Francois Bissonnette [mailto:[log in to unmask]] > Sent: Tuesday, March 15, 2011 9:36 AM > To: Jack Crawford > Subject: Cannot go on technet... but I have a question. > > Hello M. Crawford, > > I once was a member of IPC. Since I changed company, I do not have thesame liberty and right now I find myself with a problem that I never hadbefore. > > After assembling a IC with Water Soluble flux and washing the board in hot water, I find some kind of greasy residue... looks like syrup a little bit. It does not seem to dry over a few days. I have no clue and likeI said, I don't have access to Technet at the moment. (cie policy). > > Important ICs are hand soldered and hand washed with a brush under the hottest water possible. They are dried with compressed air. The residuedoes not show up anywhere else than around the IC. > > Would you have any idea on what it is and/or how to confirm what it is? > > Thanks a million! > > Jean-Fran�ois Bissonnette > DEPRO �lectronique Inc > 755, Cur�-Boivin suite 101 > Boisbriand, Qu�bec > Canada J7G 2J2 > Ph. 450.430.6251 Poste/Ext: 109 > Fax: 450.430.6251 > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________