Dave is on to something there! If they had trouble with something as simple as keeping the copper where the artwork says it should be, what else is wrong? The defect you described could be isolated, but it could also indicate a process problem, which could indicate that the fabricator isn't very careful, meaning you might find more problems. I've gone through a bunch of vendor qualification efforts recently, as supply chain tries to save money by buying defective boards. Almost every time that I find some passable process indicator, I find other defects when looking closer. Pete --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------