Cedric, I agree with Paul that the solder paste is the biggest contributor to voiding. So back to my original suggestion, can you pre-tin the bottom of the power transistor, and pre-tin the nickel-plated area on the aluminum, then reflow with a thin sheen of tacky flux such as Alpha WS319? Perhaps you do not even need to pre-tin the nickel-plated aluminum substrate, the solder on the bottom of the power transistor should be enough. This will greatly reduce the amount of voiding seen. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards Sent: Thursday, February 17, 2011 2:37 PM To: [log in to unmask] Subject: Re: [TN] Voids issue on Aluminium base plate First question is how much voiding is acceptable and what is an acceptable distribution? When bonding machined or cast Al substrates to flat surface with solder paste you will always get voids except when you do it in a vacuum furnace... The big problem is solder paste is ~50% flux so unless you "pump" the flux out of the joint material you will have voids... Where you have them and how big they are area function of size of the bonding area, surface finish, surface roughness, surface planarity, solder paste placement, solder paste type and reflow profiles... You have to remember that in the best case, at reflow temperatures that reflowed paste is a high density fluid mixed with pockets of up to 30% the same volume of low density fluid trapped between 2 parallel plates. SO the question is back to "where do voids cause the least harm?"... If the top surface of the joint had a slight upward taper(or radius) with "radial grooves" such that the "groove" depthXwidth product increase toward the outside then the trapped fluids could flow to the outside of the joint.. Also if you coat the surface with a gradual increasing thickness of something like an OSP or a high melting point organic material with gas relief channels, the molten solder would wet to the center of the joint area and progress outward as the OSP/high melting point material releases exposing base metal solder to the solder melt. As long as the solder melt wets to the top surface of the joint starting from the inside and moving out, the wetting front should push the flux and gases out of the joint in front of the bulk solder melt. Paul Paul Edwards Process/Quality Engineering Surface Art Engineering -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Cedric ORAIN Sent: Thursday, February 17, 2011 11:53 AM To: [log in to unmask] Subject: Re: [TN] Voids issue on Aluminium base plate George, It is in a recessed cavity. Regards, Cedric -----Message d'origine----- De : TechNet [mailto:[log in to unmask]] De la part de Wenger, George M. Envoyé : jeudi 17 février 2011 17:48 À : [log in to unmask] Objet : Re: [TN] Voids issue on Aluminium base plate Cedric, What is the size of the RF transistor base? Is the transistor on a flat aluminum surface or is it in a recessed cavity on an aluminum chassis? Regards, George George M. Wenger Senior Principal Reliability / FMA Engineer Andrew Corporation - Wireless Network Solutions 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 Office (732) 309-8964 Mobile E-mail: [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Bavaro Sent: Thursday, February 17, 2011 11:27 AM To: [log in to unmask] Subject: Re: [TN] Voids issue on Aluminium base plate Cedric, Lots of things come to mind....plating thicknesses, paste patterns, wetting, profiles. Is there any pattern to the voiding? Does it resemble the printed paste shape? I have soldered lots of RF transistor bases down, but I haven't ever soldered them to NiAg plated aluminum (always to Ni/Au plated copper slugs). You don't mention the paste patterns used but that will contribute to large voiding if you don't give the gases a path to get out. I would reduce the solder paste coverage to 45%, use a checkerboard pattern of dots, and then observe the voiding pattern. This assumes that the voiding is not relative to wetting as that will change everything. To do this, check the solderability of both surfaces being soldered to independently. Phil -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Cedric ORAIN Sent: Thursday, February 17, 2011 6:26 AM To: [log in to unmask] Subject: [TN] Voids issue on Aluminium base plate Dear Technetters, We have to solder a RF power transistor onto an aluminium base plate and we are facing with a very challenging issue. We encountered a high voids rate (>30% or 40%) underneath the component body (which is about 35x10mm). This is not acceptable for this application. The component is Nickel/gold plated whereas the aluminium baseplate is plated with Nickel and Silver and then cleaned with solvent. We tried to change/adapt: - soak time of the profile, - 2 difference solder pastes (SAC305), - change the screen design and thickness Finally none of these parameters looks to have significant effect on voids rate. We are now wondering if the solderability of the Ni/Ag plating is good enough and even if it is convenient for that purpose. Is somebody could give us advises? How to enhanced NiAg plating solderability (acid ?!, ...)? Which flux could help to compensate the poor wettability? Which kind of plating would be preferable? ... Thanks and regards, Cedric ---------------------------------------------------------------------------- -- This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ============================================================================== This email and any attachments thereto may contain private, confidential, and privileged material for the sole use of the intended recipient. Any review, copying, or distribution of this email (or any attachments thereto) by others is strictly prohibited. If you are not the intended recipient, please contact [log in to unmask] immediately and permanently delete the original and any copies of this email and any attachments thereto. ============================================================================== ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------