Kevin, Yes it is possible to remove Sn and then do ImAg plating. Actually many PCB fabricators use Sn as an etch relief when they fabricate circuitry on PCBs and then etch the Sn off before a final surface finish is plated. That final finish could be almost anything (e.g., ImAg, ENIG, ImSn, HASL, etc.) Regards, George George M. Wenger Senior Principal Reliability / FMA Engineer Andrew Corporation - Wireless Network Solutions 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 Office (732) 309-8964 Mobile E-mail: [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Glidden, Kevin Sent: Thursday, January 27, 2011 2:19 PM To: [log in to unmask] Subject: [TN] Re-finish ImSn to ImAg ? Question of PCB finishes... We changed specification on a PCB from ImSn to ImAg. The PCBs were built with ImSn, so we returned them. The PCB supplier is stating the ImSn was removed and they were replated with ImAg. Is this possible, or did they just plate Ag over Sn? If it IS possible, is it safe for the rest of the PCB? Thanks, Kevin ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------