Thanks
Kang. However the lead can’t bend due to there should be caused the
solder pad lift.
Thanks and best regards,
Justin Wu
Utilux South China Ltd
Phone: +86-755-2850 7521
Fax: +86-755-2850
0927
E-mail Address: [log in to unmask]
From:
TGAsia [mailto:[log in to unmask]] On Behalf Of OPR/MTD-HM/PPT
Wei Jian Kang
Sent: Saturday, December 04, 2010
8:54 AM
To: [log in to unmask]
Subject: Re: [TGAsia] Consultation
Justin
Wu:
Please
open the enclosed file for my comments.
Kang
From:
TGAsia [mailto:[log in to unmask]] On Behalf Of Justin
Wu
Sent: Friday, December 03, 2010
8:59 PM
To: [log in to unmask]
Subject: Re: [TGAsia] Consultation
Hi
All,
We found some poor solderability
on the PCB due to shifting of solder mask to cause less area of solder pad to
form a good joint. We tried to hand solder but still no good. So, would you
please help advise whether it is can be repaired?
[log in to unmask]">
Thanks in advance!
Best regards,
Justin Wu
Utilux South China Ltd
Phone: +86-755-2850 7521
Fax: +86-755-2850
0927