Hi
All,
We found some poor
solderability on the PCB
due to shifting of solder
mask to cause less area of solder pad to form a good joint. We tried to hand
solder but still no good. So,
would you please help advise
whether it is can be repaired?
Thanks
in
advance!
Best
regards,
Justin
Wu
Utilux
South China Ltd
Phone:
+86-755-2850 7521
Fax: +86-755-2850
0927
**********************************************************************
This message and any attachment are confidential and may be
privileged or otherwise protected from disclosure. If you are not the
intended recipient please telephone or e-mail the sender and delete
this message and all attachments from your system. If you are not the
intended recipient you must not copy this message or any attachment
or disclose the contents to any other person.
E-mail transmission cannot be guaranteed to be secure, error-free or
virus-free. The sender therefore does not accept liability for any
errors, omissions or consequences which arise as a result of e-mail
transmission. This message is provided for informational purposes
only and is not legally binding unless verified in writing by the sender.**********************************************************************