请教各位,是不是镀镍的表面可焊性就会稍差一些,而且焊锡流动和湿润不好?

 

 

Best regards!

Tommy Wang 王鑫

MAS Product Engineer

Laird Technologies(Beijing)Co,Ltd.

No.14,Jin Xiu Street,Bussiness Development Area,Beijing

100176,China

英资莱尔德无线通信技术(北京)有限公司

中国北京市经济开发区锦绣街14号(100176

Phone:+86 10 5933 3471

Mobile:+86 15011516577

E-mail:[log in to unmask]

Website:www.lairdtech.com

 