John Anselmo, Tape the vents with Kapton film or liquid mask then do the water-washable assembly, clean the boards then remove the tape/soldermask. The vents are there for a long term problem (venting material from the soldermask under the lid or the chemicals in the FR4 in the small pc board that is under the lid. The board is there for the bypass capacitors. A presentation by Xilinx on how they assemble their parts explains the issues. http://www.hlinstruments.com/Foresite/wp236_Flip%20chip%20package%20design_construction.pdf You can read (and see pictures) at this link about the problem http://www.hlinstruments.com/Foresite/ Bob Landman H&L Instruments, LLC www.hlinstruments.com LDF Coatings, LLC www.ldfcoatings.com -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman Sent: Friday, December 03, 2010 9:52 AM To: [log in to unmask] Subject: Re: [TN] DI Wash of Xilinx BGA Hi folks! Bill Vuono of Raytheon gave a great ppt at the IPC/SMTA Cleaning & Conformal Coating Conference a couple of weeks ago which would be a beneficial reference material for this issue. Look for the following presentation title "Resolving the Issue of Cleaning Fluid Entrapment Under Vented Flip Chip Packages" Dave Hillman Rockwell Collins [log in to unmask] John Goulet <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 12/03/2010 08:40 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to [log in to unmask] To [log in to unmask] cc Subject Re: [TN] DI Wash of Xilinx BGA To John Anselmo The Xilinx wash spec recommends baking afterwards to assure the part is dry. In practice blow out the water with an air gun to assure there is no water under BGAs, the heated board will then dry. The hot water 140-145F will safely dissolve the OA flux from the other components and posses no risk to BGAs. However from a processing time, double handling and risk damaging or knocking off bottomside SMT chip components in the wash you may want to consider putting on the post wave parts with a No-Clean flux pen. Just flux the topside holes prior to inserting the part with the flux pen. If the customer doesn't allow any No-clean residue then 3M makes an excellent cleaner that the operator can use after hand solder. The product flow continues and uses less racks etc. If you would like info on a safe cleaning mat designed for cleaning SMT boards in an in-line aqueous cleaner that prevents all of the aqueous cleaning/board handling related issues just E-mail me. John Goulet MFG/Process Engineer ----- Original Message ----- From: "John Anselmo" <[log in to unmask]> To: [log in to unmask] Sent: Thursday, December 2, 2010 11:59:53 AM Subject: [TN] DI Wash of Xilinx BGA Hi all, I have a processing question. We are building a CCA with a Xilinx 256 ball BGA. The problem is there will be some components added after the BGA is placed. Normally we used water soluble flux in hand add. Is it okay to wash the CCA's with the BGA already placed? I found some information in the archives (one email string recommending sealing the BGA to prevent water from getting under the lid). Any other issues with a DI water wash? Thanks, John ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------