Dear Yuan

 

有機型的松香經過長時間制放後確實有機會出現上述問題.

FTIR (傅立葉紅外線光譜) 這是做化合物分析時很常用的設備.

 

BR

Leo

 


From: TGAsia [mailto:[log in to unmask]] On Behalf Of yuank0
Sent: Friday, November 05, 2010 4:21 PM
To: [log in to unmask]
Subject: Re: [TGAsia] [TGAsia ]
使用有机的 焊接松香必须清洗

 

谢谢,是不是有机的在长时间下容易残留导致焊盘可能腐蚀,周围发白,什么是FTIR?谢谢你的帮组。
At 2010-11-05 13:03:25
"Frank Lan" <[log in to unmask]> wrote:

有机的是很危险,特别是-OH有活性。建议慎重考虑使用。可以用FTIR探测残余物是否含有具活性的-OH基。

 

From: TGAsia [mailto:[log in to unmask]] On Behalf Of yuank0
Sent: Friday, November 05, 2010 12:37 PM
To: [log in to unmask]
Subject: [TGAsia]
使用有机的焊接松香必须清洗

 

大家好,当使用了有机类型的焊接松香无论是否属于免洗性质的都需要清洗,否则残留的松香会存在潜在的腐蚀,如使用树脂型的免洗可以在最后免清洗,你们认为是这样的吗?谢谢




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


=======================================================================
This e-mail is intended for the person it is addressed to only. The
information contained in it may be confidential and/or protected by
law. If you are not the intended recipient of this message, you must
not make any use of this information, or copy or show it to any
person. Please contact us immediately to tell us that you have
received this e-mail, and return the original to us. Any use,
forwarding, printing or copying of this message is strictly prohibited.
No part of this message can be considered a request for goods or
services.
=======================================================================




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________