Electroplated copper before imaging helps having less variation in overall copper thickness. This is especially important when there are isolated circuitry features. Sherif -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Uppina Nagaraj Sent: Tuesday, November 02, 2010 12:16 AM To: [log in to unmask] Subject: [TN] Query on Copper plating Hi All, We have a low build electroless Copper plating for Through Hole metalization, which's giving around 0.5 to 0.6microns of Copper. The subsequent processes are pattern image printing followed by pattern plating (electrolytic copper plating). One of our customer has a requirement to do flash Copper plating (electro plating) of around 8 to 10 microns, immediately after electroless Copper plating, prior to pattern image printing. I want some inputs on the above..... Is there a distinct advantage on PTH reliability by having 8-10microns of electroplated copper immediately after electroless Copper plating. Will having additional flash plating have better Thermal stress & Thermal Shock performance. Thanks! U.Nagaraj ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------