Greetings 'netlings, I present here http://ipc-technet.groupsite.com/galleries/photo/158694 an x-ray image of a pin-in-paste thru-hole connection, SAC305 with NC on a .092" OSP SMT both sides assy with some very bothersome ground planes. My concern is we are trying to achieve 50% hole fill and 610 makes an assumption the hole is full from one side or the other. Our 5DX is happy with this assumption as well. What we have here is >50% hole fill by volume, however there is void in the middle of the joint caused by gassing of the flux. 5DX doesn't like to so well. We have had mixed results with wave and selective as the "techs" tend to compensate hole-fill difficulties (primary root cause: oxidation) by overexposure and causing Cu dissolution, sometimes to total annular ring disappearance. My question is twofold: Is 610 "interpretable" to accept >50% on Class 2 ground pins if the hole fill is not continuous, i.e., 26% from top down and 26% from bottom up, 48% void in the center?: I've noticed some holes have a "sausage" shape indicating the possibility of non-wetted hole wall and we're simply "molding" the solder into shape and not making an integral connection. If this is possibly the case, is there any non-destructive test we can do to verify integrity? Now off subject: History of Electricity was awesome! I think there should be a subchapter in the section on smoke theory to cover the electrolytic confetti generator and the noise emitting diode. Regards, Ed Popielarski Sr. Mfg. Engr. NBS Corporation 2950 Patrick Henry Dr. Santa Clara, Ca. 95054 Ph: 408-654-1100 Fx: 408-654-1107 Cl: 408-234-1497 Cl: 949-581-6601 ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------