IPC test method standards are open and no charge for download. Some parts of 2.3.26 have been superceded by 2.3.25 - and that has more than one standards section, also. Here is the current standard still left in 2.3.26: http://www.ipc.org/4.0_Knowledge/4.1_Standards/test/2.3.26.2.pdf You will have to be more specific about which cleanliness test you want. Denny Fritz -----Original Message----- From: Lamar Young <[log in to unmask]> To: TechNet <[log in to unmask]> Sent: Mon, Nov 29, 2010 10:33 am Subject: [TN] obsolete TM 650 Technetters, Does anyone have a copy of TM-650 2.3.26? know it is superseded by 2.3.25 but I've been asked for a copy of .3.26. If a copy is not available, then any information about the content of .3.26 would be helpful. Thanks, amar ______________________________________________________________________ his email has been scanned by the MessageLabs Email Security System. or more information please contact helpdesk at x2960 or [log in to unmask] _____________________________________________________________________ --------------------------------------------------- echnet Mail List provided as a service by IPC using LISTSERV 15.0 o unsubscribe, send a message to [log in to unmask] with following text in he BODY (NOT the subject field): SIGNOFF Technet o temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) o receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest earch the archives of previous posts at: http://listserv.ipc.org/archives lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for dditional information, or contact Keach Sasamori at [log in to unmask] or 47-615-7100 ext.2815 ---------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------