The scope of this method : This test method defines the procedure for determining the adhesion of solder resists (masks) used over melting metals, (such as solder plated and reflowed solder printed boards both prior to and after soldering), nonmelting metals, and printed board substrates. Says that the test is used before and after solder for only melting metals. Yet on page 2 5.1.4 Testing is to be conducted on specimens before and after soldering in accordance with J-STD-003, Methods A, B, C, or D with no accelerated aging. It says that you test a G coupon before, cut it out and do solderability testing on it and test it again. Are most people doing a before and after with SMOBC? If you are and are using a G coupon cut, fluxed and solder floated in accordance with J-STD-003,method C do you have to fixture the coupon to pull it? or just hold down the edges? What do you do if you use a production PB? Do you use it for solderability testing and adhesion test it before and after and then scrap the part? Thanks in advance Elaine Elaine Brown PWB Quality Engineering Lockheed Martin Systems Integration - Owego 1801 State Route 17C MD0409 Owego, NY 13827 Phone: 607-751-2015 FAX: 607-751-7796 e-mail: [log in to unmask] ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------