sometimes brown oxide may cause laser via reliability problem. At 2010-10-21 09:35:32£¬jan <[log in to unmask]> wrote: >Brown oxide is more popular since the simple and fast procedure according to >Original Black oxide. >But Brown oxide is poor of bonding strength than Black oxide. And for High >speed design, Brown oxide is better because of the flatness of trace. > >Best regards! >Jan Chen > >-----Original Message----- >From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Richard >Lenser >Sent: Wednesday, October 20, 2010 10:38 PM >To: [log in to unmask] >Subject: [DC] brown oxide vs black oxide > >Hi, > >Our supplier is changing their process from black oxide to brown oxide. >They >are asking us for approval. Has anyone here gone through this change? What > >are the benefits and/or problems? > >Thanks and best regards, > >Richard Lenser >Niles Audio Corporation >Miami, Florida > >---------------------------------------------------------------------------- >----- >DesignerCouncil Mail List provided as a free service by IPC using LISTSERV >1.8d >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF DesignerCouncil. >To temporarily stop/(restart) delivery of DesignerCouncil send: SET >DesignerCouncil NOMAIL/(MAIL) >Search previous postings at: www.ipc.org > On-Line Resources & Databases > >E-mail Archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 >for additional information, or contact Keach Sasamori at [log in to unmask] or >847-615-7100 ext.2815 >---------------------------------------------------------------------------- >----- > > >______________________________________________________________________ >This email has been scanned by the MessageLabs Email Security System. >For more information please contact helpdesk at x2960 or [log in to unmask] >______________________________________________________________________ > >--------------------------------------------------------------------------------- >DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d >To unsubscribe, send a message to [log in to unmask] with following text in >the BODY (NOT the subject field): SIGNOFF DesignerCouncil. >To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL) >Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives >Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 >--------------------------------------------------------------------------------- so ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________