sometimes brown oxide may cause laser via reliability problem.
At 2010-10-21 09:35:32,jan <[log in to unmask]> wrote:
>Brown oxide is more popular since the simple and fast procedure according to
>Original Black oxide.
>But Brown oxide is poor of bonding strength than Black oxide. And for High
>speed design, Brown oxide is better because of the flatness of trace.
>
>Best regards!
>Jan Chen
>
>-----Original Message-----
>From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Richard
>Lenser
>Sent: Wednesday, October 20, 2010 10:38 PM
>To: [log in to unmask]
>Subject: [DC] brown oxide vs black oxide
>
>Hi,
>
>Our supplier is changing their process from black oxide to brown oxide.
>They
>are asking us for approval. Has anyone here gone through this change? What
>
>are the benefits and/or problems?
>
>Thanks and best regards,
>
>Richard Lenser
>Niles Audio Corporation
>Miami, Florida
>
>----------------------------------------------------------------------------
>-----
>DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
>1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
>To temporarily stop/(restart) delivery of DesignerCouncil send: SET
>DesignerCouncil NOMAIL/(MAIL)
>Search previous postings at: www.ipc.org > On-Line Resources & Databases >
>E-mail Archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>----------------------------------------------------------------------------
>-----
>
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------------------------------------
>DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
>To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
>Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>---------------------------------------------------------------------------------
so
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________