I don't like to check samples which were "presolderd" by suppliers. Usually, I request a board which failed due to only cosmetic reasons or, if not available I sacrifice a good board if possible. Some resons are: I don't know if the solderability test was done according to the requirements of IPC; I don't know how my actual boards will do after shipping and storage; I don't know how the surface solderability will be for printing and reflow; I don't know if the solder alloy was SN/PB or lead free- although an experienced eye ca distinguish it; I usually prefer to choose the areas I want to check; I want to see if there are differences between before and after; And more others. Lately the purchasing department is not happy with requiring one more board for testing, but we need anyway a board for profiling, and sometimes I can use it. Good luck! Gaby -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Reid Sent: ו 01 אוקטובר 2010 17:40 To: [log in to unmask] Subject: Re: [TN] Microsection Hi Wee, Microsections (XS) do take awhile to learn how to read and Ian is very accomplished at XS interpretation. From a quality point of view you can review copper thicknesses, line width, hole roughness, drill smear, nail heading, etch back and the list goes on, and on. You get a good insight on many process steps used to fabricate PWBs, but that comes with experience. The industry processes microsections on any number of planes, through any number of structures, to find out different things about the board. A vertical section through the via is most common. Horizontal sections help understand registrations and on occasion find CAF (Ian did once). My area of expertise is in understanding the reliability implications of failed vias. You may find my column Reid on Reliability in iconnect007 useful. Here is a link to a column on PTH wear out. http://www.pcb007.com/pages/zone.cgi?a=58530&artpg=1&topic=0 The column will link to other columns that address interpretation of failed coupons by means of microsections. Sincerely, Paul Reid Program Coordinator PWB Interconnect Solutions Inc. 235 Stafford Rd., West, Unit 103 Nepean, Ontario Canada, K2H 9C1 613 596 4244 ext. 229 Skype paul_reid_pwb [log in to unmask] <mailto:[log in to unmask]> -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ian Hanna Sent: October 1, 2010 10:41 AM To: [log in to unmask] Subject: Re: [TN] Microsection Wee Mei -- Vias typically represent worst-case drilling and plating and are a good indication of the overall board build quality...I would think they were doing you a favour. In my former life as quality in a fab house I would examine vias for my internal purposes, but forward the larger PTH as part of the microsection puck unless otherwise specified by my customers -- Cheers -- Ian Lum Wee Mei <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 10/01/2010 10:35 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Lum Wee Mei <[log in to unmask]> To [log in to unmask] cc Subject [TN] Microsection With regard to PCB microsection, is it a must that microsection has to be done on plated through holes. I received a pre- and post microsection samples from my vendor and noticed that they are done across the plated through via. Of course, the solder cannot flow through the walls of the vias on the post solder sample. Can I accept this post solder sample and use it to verify the fabrication process? If yes, what are the reasons. I am learning the trade by myself and would appreciate I can learn from the experts in the field. If there is any articles on how to interpret the microsection sample for PCB such how to differentiate electroless copper from copper plating and then the tin-lead plating in the wall or pad surface, etc would also be most appreciated. Thanks and Regards, ~ Wee Mei ~ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- __________ Information from ESET NOD32 Antivirus, version of virus signature database 5496 (20101001) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com __________ Information from ESET NOD32 Antivirus, version of virus signature database 5496 (20101001) __________ The message was checked by ESET NOD32 Antivirus. http://www.eset.com ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------