We do not use OSP finish here at GD. However, we do use it at my other client companies. I will find out which OSP product it is and get back to you tomorrow. dean -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo Sent: Monday, October 18, 2010 4:00 PM To: [log in to unmask] Subject: Re: [TN] Detecting Oxidation Levels of PTH What is your OSP? What is vendor recommended reflow times? What temp and for how long? (You do not have to spill the bean). The answer is in the material and process selection. Someone did not do the homework and you pay for it. -------------------------- Sent using BlackBerry ----- Original Message ----- From: Leland Woodall [mailto:[log in to unmask]] Sent: Monday, October 18, 2010 04:41 PM To: [log in to unmask] <[log in to unmask]> Subject: Re: [TN] Detecting Oxidation Levels of PTH Joyce and Richard, Even though we have our upper thresholds set at 500 PPM, we consistently run these specific lines between 35 and 70 PPM. The most capable (and newest) reflow ovens we have are producing the problem product. Which only adds to the mystery... Leland -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo Sent: Monday, October 18, 2010 4:23 PM To: [log in to unmask] Subject: Re: [TN] Detecting Oxidation Levels of PTH However, he need to preserve what ever the OSP left in the hole and prevent the oxidation prior to hit the wave. The 100ppm or less for the SMT 2x is important if it is not criticle. What ever it is, the 500ppm is the down fall for sure. -------------------------- Sent using BlackBerry ----- Original Message ----- From: Stadem, Richard D. [mailto:[log in to unmask]] Sent: Monday, October 18, 2010 02:24 PM To: [log in to unmask] <[log in to unmask]> Subject: Re: [TN] Detecting Oxidation Levels of PTH Agree. However Leland was talking about the reflow ovens, not the wave solder, which led to my posting. I agree however that Nitrogen levels don't do a lot for a turbulent wave. From: Paul Edwards [mailto:[log in to unmask]] Sent: Monday, October 18, 2010 11:46 AM To: TechNet E-Mail Forum; Stadem, Richard D. Subject: RE: [TN] Detecting Oxidation Levels of PTH For SMT under around 100ppm gives sometimes gives great results, but haven't seen the less than the 500 ppm grive radical improvement in wave solder because of the turbulence of the wave and activity of the flux... Paul Paul Edwards Surface Art Engineering -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Saturday, October 16, 2010 6:02 AM To: [log in to unmask] Subject: Re: [TN] Detecting Oxidation Levels of PTH Oxygen levels should be less than 75 ppm, else don't bother. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall Sent: Friday, October 15, 2010 7:45 AM To: [log in to unmask] Subject: Re: [TN] Detecting Oxidation Levels of PTH Joyce, We have nitrogen in the reflow ovens with max O2 levels of 500 ppm. Our facility humidity is controlled and within a range of 35 to 45%. We also have nitrogen pumping at the wave bath. Leland -----Original Message----- From: Joyce Koo [mailto:[log in to unmask]] Sent: Friday, October 15, 2010 8:37 AM To: [log in to unmask]; Leland Woodall Subject: Re: [TN] Detecting Oxidation Levels of PTH Not nitrogen reflow prior to wave? How many times SMT before wave? What is the humidity contorl on the floor? -------------------------- Sent using BlackBerry ----- Original Message ----- From: Leland Woodall [mailto:[log in to unmask]] Sent: Friday, October 15, 2010 08:32 AM To: [log in to unmask] <[log in to unmask]> Subject: Re: [TN] Detecting Oxidation Levels of PTH OSP over copper, lead-free, SAC 305 process. -----Original Message----- From: Tan Geok Ang [mailto:[log in to unmask]] Sent: Thursday, October 14, 2010 8:23 PM To: TechNet E-Mail Forum; Leland Woodall Subject: RE: [TN] Detecting Oxidation Levels of PTH ImAg Boards? -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall Sent: Friday, 15 October 2010 3:49 AM To: [log in to unmask] Subject: [TN] Detecting Oxidation Levels of PTH Techies, We have one assembly that sporadically experiences insufficient solder fill of plated through holes at the wave soldering process. If we cross section one of these, what testing equipment is best suited to detect the presence of oxidation on the PTH walls? What would be considered an unacceptable level that would prevent 100% climb? Thanks in advance for your responses! Leland ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ________________________________ This email and any attachments thereto may contain private, confidential, and privileged material for the sole use of the intended recipient. Any review, copying, or distribution of this email (or any attachments thereto) by others is strictly prohibited. If you are not the intended recipient, please contact [log in to unmask]<mailto:[log in to unmask]> immediately and permanently delete the original and any copies of this email and any attachments thereto. ________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------