Hi

如果有图解看你们的操作会更明白,我们是手工焊接,如果只是固定和焊接相信你们会摸索出来解决的

 

 

Best regards

Jenny 李清荣

/:  No. 569 Xuhua Road Xujing Town Shanghai P.R. China

(:   +86 021-59761331 ext.109

*: [log in to unmask]

 

发件人: TGAsia [mailto:[log in to unmask]] 代表 Wood Fang [LTBJ]
发送时间: 2010928 11:20
收件人: [log in to unmask]
主题: Re: [TGAsia] 如何手工焊接细COAXIAL cable

 

HiMark

 我们是想把COAXIAL CABLE  焊接到FLEX FILE 软板上, 但是固定和焊接总是有问题。

你们是手工还是自动?

 

wood fang

mechanical engineer,Lairdtech,Beijing

86-10-59333595

8613146882520

Add. No.14, Jinxiu Street, Beijing Development Area, China

 

From: Mark Yang [mailto:[log in to unmask]]
Sent: 2010
928 11:16
To: Asia Committe Task Group Forum; Wood Fang [LTBJ]
Subject: Re: [TGAsia]
如何手工焊接细COAXIAL cable

 

HiWood

 

您可以外发给良特电子来加工的,专业生产同轴线缆组装加工!

 

http://www.exceltek.com.cn

 

----- Original Message -----

From: [log in to unmask]">Wood Fang [LTBJ]

To: [log in to unmask]">[log in to unmask]

Sent: Tuesday, September 28, 2010 10:50 AM

Subject: [TGAsia] 如何手工焊接细COAXIAL cable

 

 

Hi, all

如何手工焊接细COAXIAL cable

谢谢

wood fang

mechanical engineer,Lairdtech,Beijing

86-10-59333595

8613146882520

Add. No.14, Jinxiu Street, Beijing Development Area, China

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


__________ Information from ESET NOD32 Antivirus, version of virus signature database 5484 (20100927) __________

The message was checked by ESET NOD32 Antivirus.

http://www.eset.com


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________